Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 200 °C | 392 °F | |
Premix Thermoplastics PRESEAL® TPE 5010 PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica.. |
|||
Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The .. |
|||
Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Nozzle Temperature | 200 - 232 °C | 392 - 450 °F | Average value: 220 °C Grade Count:15 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Nozzle Temperature | 200 - 210 °C | 392 - 410 °F | Injection |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Nozzle Temperature | 200 - 210 °C | 392 - 410 °F | Injection |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Nozzle Temperature | 200 °C | 392 °F | |
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Nozzle Temperature | 200 °C | 392 °F | |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Nozzle Temperature | 200 °C | 392 °F | |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Nozzle Temperature | 200 °C | 392 °F | |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Nozzle Temperature | 200 °C | 392 °F | |
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |