Polymer Property : Nozzle Temperature = 210 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Oxford Polymers C-Acetal 25GF-BK Acetal, 25% Glass Fiber Reinforced
Product Description: Glass Fiber (25% Reinforced), Acetal Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristics: Pre-color..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic..
Nozzle Temperature 195 - 210 °C
383 - 410 °F
Huntsman AVALON® 60 DE Thermoplastic Polyurethane
Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
Injection
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Nozzle Temperature 185 - 210 °C
365 - 410 °F
Injection
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT..
Nozzle Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
Stellarchem DIOSHY® MP-960NC TPE Compound
This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1221A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1267A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2519G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2550A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2596B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2683B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-6075 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-83-F912-G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-2683D Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Teknor Apex Telcar® TL-91-T3056S-90 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..