Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 190 - 215 °C | 374 - 419 °F | |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 190 - 215 °C | 374 - 419 °F | |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
Nozzle Temperature | 195 - 215 °C | 383 - 419 °F | Injection Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 190 - 215 °C | 374 - 419 °F | |
LG Chemical Lucet® N109 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 190 - 215 °C | 374 - 419 °F | |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection Molding |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |
|||
Nozzle Temperature | 185 - 215 °C | 365 - 419 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | |
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | |
Lubrizol Estane® S195A Thermoplastic Polyurethane Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | |
Lubrizol Estane® L194A Thermoplastic Polyurethane Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan.. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 200 - 215 °C | 392 - 419 °F | Injection |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Nozzle Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |