Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS E112LG Pellets Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H604 ABS Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® M205FC ABS Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® 5300 ABS Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | |
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled 5 % mineral filledfor thin-wall applicationsinjection moldingVicat/B 120 = 103 °CHDT/A = 85 °Cvery good UL listing in small wall thickness (V-0 at 0.75 mm)PreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled 15 % mineral filledinjection molding gradeincreased stiffnesstensile modulus = 4800 MPaVicat/B 120 temperature = 98 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame ret.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3010 IF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3015 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3200 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T50 XF Polycarbonate + ABS Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T90 HT Polycarbonate + ABS Injection molding gradehigh heat resistanceVicat/B 120 = 135 °Cball indentation temperature = 125 °Ceasy flowsuitable for supporting life componentsPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T95 MF* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade9 % mineral filledvery high heat resistancereduced coefficient of linear thermal expansiontensile modulus = 3350 MPaVicat/B 120 = 142 °CPreprocessingMax... |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |