Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 240 mm/sec | 9.45 in/sec | |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS E112LG Pellets Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® 4115 ABS Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® E309 ABS Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® 5300 ABS Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3011 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegood flowhigh heat resistanceVicat/B 120 temperature = 118 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled 5 % mineral filledfor thin-wall applicationsinjection moldingVicat/B 120 = 103 °CHDT/A = 85 °Cvery good UL listing in small wall thickness (V-0 at 0.75 mm)PreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3010 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3110 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T45 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T90 HT Polycarbonate + ABS Injection molding gradehigh heat resistanceVicat/B 120 = 135 °Cball indentation temperature = 125 °Ceasy flowsuitable for supporting life componentsPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |