Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Manufacturer Polymer Resources, LTD
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Melt Flow 5.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 250 °C
5.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
ASTM D638
Tensile Strength, Yield 124 MPa
18000 psi
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature 22.8 °C
1.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0626 in
HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
Processing Properties Metric English Comments
Rear Barrel Temperature 238 - 254 °C
460 - 490 °F
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Front Barrel Temperature 249 - 266 °C
480 - 510 °F
Melt Temperature 232 - 260 °C
450 - 500 °F
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Drying Temperature 116 - 121 °C
240 - 250 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Descriptive Properties Value Comments
Vent 0.0005