Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5300M PBT+PC+MF30% Description: Injection Molding, PBT+PC+MF30%, Low WarpageApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 103598-77-2, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3250A PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2303 PBT+GF30% Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, DRY Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
Front Barrel Temperature | 250 - 255 °C | 482 - 491 °F | |
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 240 - 255 °C | 464 - 491 °F | |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Solvay TECHNYL® C 52G3 MZ25 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosph.. |
|||
Front Barrel Temperature | 240 - 255 °C | 464 - 491 °F | |
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America.. |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | |
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin 30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |