Front Barrel Temperature 246 - 279 °C
475 - 535 °F
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced
PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 246 - 268 °C
475 - 515 °F
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 246 - 279 °C
475 - 535 °F
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade
Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade
ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® M5372 High Density Polyethylene
ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. ..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case..
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Injection Molding
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Injection Molding
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Front Barrel Temperature 246 °C
475 °F
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade
ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys..
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Front Barrel Temperature 246 - 288 °C
475 - 550 °F
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow
Information provided by Star Plastics, Inc.
Front Barrel Temperature 246 - 266 °C
475 - 510 °F
Star Plastics PC/PBT7804 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
Front Barrel Temperature 246 - 268 °C
475 - 515 °F
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio..
Front Barrel Temperature 246 - 274 °C
475 - 525 °F
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer
X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled..
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Calsak CS-72 General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Front Barrel Temperature 246 - 268 °C
475 - 515 °F
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
Copyright © lookpolymers.com All Rights Reserved