| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Teknor Apex Company |
| Trade Name | Chemlon® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 114 MPa | 16500 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Strength | 162 MPa | 23500 psi | ASTM D790 |
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
| Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 188 °C | 370 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB @Thickness 0.810 mm |
HB @Thickness 0.0319 in |
|
| Oxygen Index | 22 % | 22 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
280 kV/in @Thickness 0.118 in |
ASTM D149 |
| Comparative Tracking Index | 500 V | 500 V | UL 746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
| Middle Barrel Temperature | 241 - 257 °C | 465 - 495 °F | |
| Front Barrel Temperature | 246 - 268 °C | 475 - 515 °F | |
| Nozzle Temperature | 246 - 268 °C | 475 - 515 °F | |
| Melt Temperature | 216 °C | 420 °F | |
| 249 - 266 °C | 480 - 510 °F | Processing Temperature | |
| Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black; Natural Color | |
| Suggested Moisture, max | 0.2 | |
| Suggested Regrind, max | 25 |