Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 3055D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 240°C |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 240°C |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Front Barrel Temperature | 230 °C | 446 °F | C5 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 206 PA6, DRY Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Front Barrel Temperature | 230 °C | 446 °F | |
Solvay TECHNYL® C 502XT PA6, DRY Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, shee.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | H3 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 280 °C | 446 - 536 °F | |
Teknor Apex Beetle® 60GS6 Nylon 6, 30% Glass Bead Reinforced, Dry Features: High rigidity and low warping. Processing Method: Injection MoldingForms: Pellets Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pr.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Pipe Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Pipe Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |