| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **)
Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 C..
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ HCA115QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **)
Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500...
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **)
Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess..
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
|
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Middle Barrel Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
|
LG Chemical LUMID GP1300AP PA6, Plasticized
Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000H PBT
Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000M PBT
Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000SB PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000W PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
|
|||
| Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® 4832 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® 901 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® 903 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® 907 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
|
Sumitomo Chemical ESPOLEX® WT515 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 175 - 245 °C | 347 - 473 °F | |
|
Equate EMDA-8920 HDPE Injection Molding Resin
EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p..
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Zone 2 |
|
Eurostar Starflam P10002E PA6, Injection Molded
Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec..
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin
20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin
30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin
Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||