Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Gichem GILAC H120X6/VOU ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0 with better fluidity and UV resistance. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa FRHIPS-117 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa FRHIPS-960 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier .. |
|||
Middle Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Start Point: 225°C |
Kingfa JH950-402 Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a.. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Middle Barrel Temperature | 180 - 230 °C | 356 - 446 °F | Injection |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform.. |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa FRHIPS-100 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud.. |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL LW4302 PP+GF/MF30% Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL LW4405 PP+GF/MF40% Description: Injection Molding, PP+GF/MF40%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 65997-17-3 and 12001-26-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | H2 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Borealis HA104E Polypropylene Homopolymer HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica.. |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |