| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 205 - 215 °C | 401 - 419 °F | |
| Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-113 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-117 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-220 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-960 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier .. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Middle Barrel Temperature | 205 - 225 °C | 401 - 437 °F | Injection Molding |
| LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Middle Barrel Temperature | 205 - 225 °C | 401 - 437 °F | Injection Molding |
| LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
| Middle Barrel Temperature | 205 - 215 °C | 401 - 419 °F | |
| Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
| Middle Barrel Temperature | 205 - 215 °C | 401 - 419 °F | |
| Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-100 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPS-930 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec.. |
|||
| Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
| Kingfa FRHIPSV-0 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud.. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | |
| SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | |
| SK Chemicals SKYTHANE® S168D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | |
| SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | Compress zone |
| Taiwan PU Corporation TPUI-T64D Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
| Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
| Sumitomo Chemical ESPOLEX® 4832 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
| Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
| Sumitomo Chemical ESPOLEX® 4855 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
| Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
| Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | Injection |
| Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | Injection |
| Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | Injection |
| Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Middle Barrel Temperature | 205 °C | 401 °F | Injection |
| Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||