| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm <br>@Thickness 3.20 mm |
0.0090 - 0.013 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 10 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
10 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 29.4 MPa <br>@Thickness 3.20 mm |
4270 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 45 % <br>@Thickness 3.20 mm |
45 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 39.2 MPa <br>@Thickness 6.40 mm |
5690 psi <br>@Thickness 0.252 in |
30mm/min; ASTM D790 |
| Flexural Modulus | 2.45 GPa <br>@Thickness 6.40 mm |
356 ksi <br>@Thickness 0.252 in |
30mm/min; ASTM D790 |
| Izod Impact, Notched | >= 0.343 J/cm <br>@Thickness 6.40 mm,<br> Temperature -10.0 °C |
>= 0.643 ft-lb/in <br>@Thickness 0.252 in,<br> Temperature 14.0 °F |
ASTM D256 |
| >= 0.588 J/cm <br>@Thickness 6.40 mm,<br> Temperature 23.0 °C |
>= 1.10 ft-lb/in <br>@Thickness 0.252 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 137 °C <br>@Thickness 3.20 mm |
279 °F <br>@Thickness 0.126 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
| Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Front Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |