Processing Properties Metric English Comments
Middle Barrel Temperature 371 °C
700 °F
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber
KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
Middle Barrel Temperature 371 °C
700 °F
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Middle Barrel Temperature 371 - 421 °C
700 - 790 °F
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Copyright © lookpolymers.com All Rights Reserved