Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Adapter Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**) Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA95MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95MP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA95QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95QP is a lubricated medium viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95YP is a lubricated medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA95ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95ZP is a medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It p.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |
|||
Adapter Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA) Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce.. |
|||
Adapter Temperature | 250 °C | 482 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Adapter Temperature | 250 °C | 482 °F | Cast Film |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Adapter Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |