Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | Mono-extrusion |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | Mono-extrusion |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Adapter Temperature | 175 - 216 °C | 347 - 421 °F | Average value: 193 °C Grade Count:41 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Adapter Temperature | 175 - 190 °C | 347 - 374 °F | |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Adapter Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Adapter Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Adapter Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Adapter Temperature | 175 - 185 °C | 347 - 365 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Adapter Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Adapter Temperature | 175 - 195 °C | 347 - 383 °F | Extrusion |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |