Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 25.0 °C | 77.0 °F | |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Feed Temperature | 25.0 °C | 77.0 °F | |
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 DB Thermoplastic Polyurethane Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |