Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant PA131 Nylon 66, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BR2025 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA112 Nylon 66, Nucleated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA211N40 Nylon 6, Mineral/Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0003 Nylon 6, High Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0004 Polycarbonate Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol TES3050A Thermoplastic Elastomer Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol TPU2087AFR Polyurethane Elastomer, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6608G43 Nylon 66, 43% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 138 MPa | 720 - 20000 psi | Average value: 43.2 MPa Grade Count:3 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |