Clariant Renol TES3050A Thermoplastic Elastomer Alloy

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol TES3050A Thermoplastic Elastomer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
ASTM D955
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.45 MPa
500 psi
ASTM D638
Flexural Modulus 0.00214 GPa
0.310 ksi
100% Modulus; ASTM D790
0.00345 GPa
0.500 ksi
300% Modulus; ASTM D790
Compression Set 29 %

@Temperature 73.0 °C,
Time 79200 sec
29 %

@Temperature 163 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Melt Temperature 193 - 221 °C
380 - 430 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm