Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.700 - 0.900 W/m-K | 4.86 - 6.25 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® 1002 Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® SMT-B-1 LAS (146.408) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It is formulated .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® 150.401 Encapsulation Resin
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A second generation SMT-B family product. This material is the initial developmental, general purpose SMT-B encapsulation grade .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | DIN 52612 |
Fluorseals PTFE 25% carbon filled Improved compressive strength, wear resistance and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 250 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 482 °F |
|
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 100 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | ASTM E1225 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 200 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
DIN 52612 |
Brandenburger ISOFLEX AFV Foam This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio.. |