Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1501 Polyester, Briquette, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1501 Polyester, Briquette, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength values. UL recognized under component file E40654. 01501 is available in gray, blue, or tan color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Density 1.89 g/cc
0.0683 lb/in³
ASTM D792
Water Absorption 0.299 %
0.299 %
ASTM D570
Linear Mold Shrinkage 0.0031 cm/cm
0.0031 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 70
70
ASTM D785
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 0.57 %
0.57 %
ASTM D638
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 10.8 GPa
1570 ksi
ASTM D790
Compressive Strength 153 MPa
22200 psi
ASTM D695
Izod Impact, Notched 0.248 J/cm
0.465 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.265 J/cm²
1.26 ft-lb/in²
ASTM D256
Impact 137
137
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.700 W/m-K

@Temperature 100 °C
4.86 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 167 °C
333 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 24 %
24 %
ASTM D2863
Shrinkage 0.043 %
0.043 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+14 ohm-cm
3.20e+14 ohm-cm
ASTM D247
Dielectric Constant 5.3
5.3
ASTM D150
Dielectric Strength 10.3 kV/mm
262 kV/in
Step by Step; ASTM D149
12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Dielectric Breakdown 20200 V
20200 V
1hr 94C; ASTM D149
Dissipation Factor 0.0278
0.0278
ASTM D150
Arc Resistance 190 sec
190 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638
Users viewing this material also viewed the following: