Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Menzolit
Trade Name Menzolit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets the demands of DIN 16913 and is classified as type 831 (831.5) regarding mechanical properties. The flammability meets the demands of standard UL 94 category HB. The glass content is on a level that combines good mouldability with good mechanical properties regarding strength and stiffness.Information Provided by Menzolit
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa

@Temperature 22.0 °C
8700 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Tensile Strength, Yield 60.0 MPa

@Temperature 22.0 °C
8700 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Modulus of Elasticity 12.0 GPa
1740 ksi
25mm flat samples, compression moulded; ISO 527-4
Flexural Strength 146 MPa

@Temperature 22.0 °C
21200 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa

@Temperature 22.0 °C
1450 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
0.30
Shear Modulus 4.60 GPa
667 ksi
in plane
Charpy Impact, Notched 6.60 J/cm²
31.4 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 170 °C
338 °F
ISO 11357-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 25 %
25 %
ISO 4589-2
Glow Wire Test 850 °C
1560 °F
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 24.0 kV/mm
610 kV/in
IEC 60243-1
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 150 °C
275 - 302 °F
Compression moulding, matched metal die