Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Thermal Conductivity | 0.260 - 0.988 W/m-K | 1.80 - 6.86 BTU-in/hr-ft²-°F | Average value: 0.527 W/m-K Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Solvay Chemicals Polyglycerol-3 A polyglycerol characterized by a very narrow oligomer distribution centered on triglycerol.EINECS Number: 915-741-3/CAS Number: 25618-55-7Information provided by Solvay |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East) PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN2V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2V is a 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® LC 350 Si Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon CP-PC-2959 Silicone Product Use: Traction motor insulation compound, electrical insulationAppearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to writ.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PAI Polyamideimide Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |