Download PDF Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough materials, highly resistant to contamination, and will not be affected by other chemicals during cure or after. Typical uses: Electronic assemblies and components.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Viscosity 16000 cP

@Temperature 25.0 °C
16000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength, Ultimate 2.65 MPa
384 psi
Elongation at Break 170 %
170 %
Tear Strength 3.80 kN/m
21.7 pli
Die B
Thermal Properties Metric English Comments
CTE, linear 220 µm/m-°C

@Temperature 20.0 °C
122 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 3.6

@Frequency 1000 Hz
3.6

@Frequency 1000 Hz
Dielectric Strength 20.5 kV/mm

@Thickness 1.90 mm
521 kV/in

@Thickness 0.0748 in
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Cure time 24 hrs.
Pot Life 90.0 min

@Temperature 25.0 °C
90.0 min

@Temperature 77.0 °F