Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Flexural Modulus 2.93 GPa
425 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.4 µm/m-°C
23.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149