Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East) GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 213 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 213 °F | ASTM D648 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ASTM D648 |
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **) Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ISO 75-1,-2 |
Ineos ABS Lustran® SAN C Injection Molding Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ISO 75A |
Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ISO 75 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | Annealed; ISO 75-2/A |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ASTM D648 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ISO 75 |
Radici Heraform® R 350 Acetal Copolymer Standard grade for injection molding of thick wall parts, stiff-flowing, extrusion grade for tubes and sheet.Information provided by Radici group. |