Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Nilit FRIANYL B63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Nilit RECONYL B S Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Nilit FRIANYL B63 H Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Qualchem Danaprop PP1GF-30 Polypropylene, 30% Glass Fiber Polypropylene (co-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
Covestro Apec® 1705 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DAM; ASTM D648 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Kolon SPESIN® KP513MT25 G/F Reinforced PBT Alloy Resin High flow, dimensionally stableApplications: Head lamp bezelsInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LG Chemical LUCEL FW-700A Friction and Wear Resistant POM, Polymeric Wear Additive LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX100 PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO 0150 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamTal PM1109 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamSter PF713 PBT, UV Stabilized UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamTal PM1609 Acetal, Molybdenum Disulfide Filled Molybdenum disulfide filled polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Staramide R1000IX2 PA66, Impact Modified, Injection Molded Staramide R1000IX2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as Star X 1010)Information provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM Test |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Cheng Yu Plastic FV30G10 POM, 10% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |