Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamSter PF713 PBT, UV Stabilized

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamSter PF713 PBT, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
DIN 53479
Water Absorption 0.60 %
0.60 %
DIN 53495
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23° C, 50% RH; DIN 53714
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 250 °C
30 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM-D638
Elongation at Break 30 %
30 %
ASTM-D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM-D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Glow Wire Test 750 °C
1380 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
DIN 53482
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4