Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact modified Nylon 6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption at Saturation 8.0 %
8.0 %
ISO 62
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
Tensile Modulus 1.89 GPa
274 ksi
ISO 527
Flexural Modulus 1.60 GPa
232 ksi
ISO 178
Izod Impact, Notched (ISO) 6.20 kJ/m²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
ISO 180
35.0 kJ/m²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.540 J/cm²

@Temperature -30.0 °C
2.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IEC 60250