Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | DIN 53461; ASTM D648 |
Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C @Thickness 3.20 mm |
435 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C @Thickness 3.20 mm |
435 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® HTN 05007 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East) LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
Cheng Yu Plastic N6GV15 Flame Retardant Nylon 6, 15% Glass Filled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ASTM D648 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ISO 75-2 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 224 °C | 435 °F | ISO 75-1,-2 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |