Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® HTN 05007

Category Polymer , Thermoplastic , Nylon , High Temperature Nylon
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® HTN 05007.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.25 %

@Time 86400 sec
0.25 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 84.6 µm/m-°C
47.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 224 °C
435 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257