Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C @Thickness 6.35 mm |
379 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | DIN 53461 |
Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C @Thickness 6.35 mm |
379 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NJC-6000 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 - 235 °C | 380 - 455 °F | Average value: 216 °C Grade Count:3 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C @Thickness 6.40 mm |
379 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/12 01430 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C @Thickness 6.40 mm |
379 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | ASTM D648 |
Chase Plastics CP Pryme® N100MD2 (COND, 50% RH) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
Unitika M2350 PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
Adell AS-10 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
Ashley Polymers Ashlene® 527 Nylon 66 A very high impact, slightly lubricated, nylon resin.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
Adell AS-30 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ISO 75 |
BASF Ultradur B 4406 G4 BKQ113 7110 20% Glass Filled PBT Ultradur B 4406 G4 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 20% glass fiber reinforcement. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 663 Nylon 6, Glass Bead Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp PK0069 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0069 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |