Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ashley Polymers Ashlene® 527 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A very high impact, slightly lubricated, nylon resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256
1.50 J/cm

@Temperature -40.0 °C
2.81 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 249 °C
480 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
379 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
ASTM D150