Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
DIN 53479
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
50 mm/min; ISO 527-1,2
Elongation at Break 3.0 %
3.0 %
ISO 527-1,2
Tensile Modulus 20.3 GPa
2940 ksi
ISO 527-1,2
Flexural Modulus 10.0 GPa
1450 ksi
DIN 53452
Charpy Impact Unnotched 3.30 J/cm²

@Temperature 23.0 °C
15.7 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
379 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
379 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 20000 ohm-cm
20000 ohm-cm
DIN 53482
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714
Users viewing this material also viewed the following: