| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
| Moisture Absorption at Equilibrium | 2.8 % | 2.8 % | 50% RH |
| Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.20 mm |
0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 88.0 MPa | 12800 psi | ASTM D638 |
| Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
| Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
| Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
| Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 147 °C | 297 °F | ASTM D648 |