Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® ML3982 PC (Europe-Africa-Middle East) LEXAN ML3982 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 - 265 °C | 266 - 509 °F | Average value: 147 °C Grade Count:91 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Asia Pacific) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 6.40 mm |
266 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 6.40 mm |
266 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 6.40 mm |
266 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
JPJ Technologies PP HC9012-M PP Homopolymer Injection Molding Information provided by JPJ Technologies |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 6.40 mm |
266 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | |
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene Characteristic: 30%wt of Sulfate Barium filled, high gloss, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GFN2V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2V is a 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ISO 75-1/-2 |
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled Injection molding grade10 % glass fiber filledtensile modulus = 3900 MPaVicat/B 120 temperature = 131 °CPreprocessingMax. Water content |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20 H FR PA12 FR Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0339W40L1 Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
Ashley Polymers Ashlene® D930H Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C @Thickness 6.40 mm |
266 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | ASTM D648 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |