Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer SPS Guang Zhou
Trade Name FILLMA™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristic: 30%wt of Sulfate Barium filled, high gloss, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 16 g/10 min
16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Flexural Strength 45.0 MPa
6530 psi
Flexural Modulus 2.20 GPa
319 ksi
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Flammability, UL94 HB
HB