Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murylon® A Nylon 66
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than..
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..
CTE, linear 80.0 - 95.0 µm/m-°C

@Temperature 25.0 - 100 °C
44.4 - 52.8 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM D696
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
CTE, linear 80.0 µm/m-°C

@Temperature <=61.0 °C
44.4 µin/in-°F

@Temperature <=142 °F
below Tg
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 100 °C
44.4 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murylat® Polyethylene Terephthalate
Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an..
CTE, linear 80.0 µm/m-°C

@Temperature >=143 °C
44.4 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 50.0 °C
44.4 µin/in-°F

@Temperature -22.0 - 122 °F
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 50.0 °C
44.4 µin/in-°F

@Temperature -22.0 - 122 °F
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
CTE, linear 80.0 µm/m-°C

@Temperature <=100 °C
44.4 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
CTE, linear 80.0 µm/m-°C

@Temperature 25.0 - 100 °C
44.4 µin/in-°F

@Temperature 77.0 - 212 °F
Horizontal; ASTM D696
Unitika UNILATE® 1 NC PET
Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a..
CTE, linear 80.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
44.4 µin/in-°F

@Temperature 122 - 158 °F
TD; ASTM D696
DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
CTE, linear 80.0 µm/m-°C

@Temperature -50.0 - 0.000 °C
44.4 µin/in-°F

@Temperature -58.0 - 32.0 °F
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
CTE, linear 80.0 µm/m-°C

@Temperature 5.00 - 30.0 °C
44.4 µin/in-°F

@Temperature 41.0 - 86.0 °F
Below Tg
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
CTE, linear 80.0 µm/m-°C

@Temperature 5.00 - 30.0 °C
44.4 µin/in-°F

@Temperature 41.0 - 86.0 °F
Below Tg
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
CTE, linear 80.0 µm/m-°C

@Temperature <=60.0 °C
44.4 µin/in-°F

@Temperature <=140 °F
below Tg
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to..
CTE, linear 80.0 µm/m-°C

@Temperature <=112 °C
44.4 µin/in-°F

@Temperature <=234 °F
below Tg
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and ..
CTE, linear 80.0 µm/m-°C

@Temperature <=112 °C
44.4 µin/in-°F

@Temperature <=234 °F
below Tg
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and ..
CTE, linear 80.0 µm/m-°C

@Temperature <=61.0 °C
44.4 µin/in-°F

@Temperature <=142 °F
below Tg
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Estimated by MatWeb from similar grades
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr..
CTE, linear 80.0 µm/m-°C

@Temperature <=55.0 °C
44.4 µin/in-°F

@Temperature <=131 °F
below Tg
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive
Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
CTE, linear 80.0 µm/m-°C

@Temperature <=60.0 °C
44.4 µin/in-°F

@Temperature <=140 °F
below Tg
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..
Copyright © lookpolymers.com All Rights Reserved