EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Alcohol (EVOH)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 2.5 %
2.5 %
Equilibrium at 65% RH
2.5 %
2.5 %
65% RH
Water Absorption at Saturation 5.0 %
5.0 %
100% RH
Moisture Vapor Transmission 0.720 cc-mm/m²-24hr-atm
1.83 cc-mil/100 in²-24hr-atm
40°C, 90% RH
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
Thickness 15.2 microns
0.600 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 260 %
260 %
10%/min.; ASTM D638
Film Elongation at Break, TD 190 %
190 %
10%/min.; ASTM D638
Secant Modulus, MD 2.00 GPa
290 ksi
Youngs Modulus, ASTM D638, 10%/min.
Secant Modulus, TD 1.90 GPa
276 ksi
Youngs Modulus, ASTM D638, 10%/min.
Elmendorf Tear Strength MD 460 g
460 g
ASTM D638
Elmendorf Tear Strength TD 440 g
440 g
ASTM D638
Elmendorf Tear Strength, MD 30.2 g/micron
767 g/mil
0.6 mil; ASTM D638
Elmendorf Tear Strength, TD 28.9 g/micron
733 g/mil
0.6 mil; ASTM D638
Film Tensile Strength at Break, MD 70.0 MPa
10200 psi
10%/min.; ASTM D638
Film Tensile Strength at Break, TD 44.0 MPa
6380 psi
10%/min.; ASTM D638
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Estimated by MatWeb from similar grades
130 µm/m-°C

@Temperature 100 °C
72.2 µin/in-°F

@Temperature 212 °F
Estimated by MatWeb from similar grades
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
Thermal Conductivity 0.340 W/m-K
2.36 BTU-in/hr-ft²-°F
For EVAL F101
Melting Point 164 °C
327 °F
DSC
Optical Properties Metric English Comments
Haze 1.7 %
1.7 %
65% RH
Gloss 90 %
90 %
65% RH
Electrical Properties Metric English Comments
Electrical Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
Surface Resistance 2.10e+15 ohm
2.10e+15 ohm
Dielectric Constant 5.5
5.5
Frequency Not Specified
Dissipation Factor 0.22
0.22
Frequency Not Specified