Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific) PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS FXC810MA is the grade code for the Marble effect in PC/ABS. Marble is part of the VisualFX portfolio, and it is offered in a range of colors simluating the Marble effect. High heat/good flow charact.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific) Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC (Asia Pacific) ASA+PC blend. Weatherable, injection grade. Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific) Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s). |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10 LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingSheet extrusionInformation provided by Bayer Polymers.As of 1 .. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |