Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 203 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 95.0 °C
203 °F
NextGen Adhesives P907-04 Fiber Optic Adhesive
Description: NGAC P907-04 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si..
Glass Transition Temp, Tg 95.0 °C
203 °F
DSC
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
Glass Transition Temp, Tg 95.0 °C
203 °F
10°C/min test
Polimeri Europa EDISTIR N1670 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP..
Glass Transition Temp, Tg 95.0 °C
203 °F
10°C/min test
Polimeri Europa EDISTIR N1671 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol..
Glass Transition Temp, Tg 95.0 °C
203 °F
ASTM D7426
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester
Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “di..
Glass Transition Temp, Tg 95.0 °C
203 °F
Eastman Tenite 105-28 Cellulose Acetate  (discontinued **)
28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 95.0 °C
203 °F
Mettler DSC
Lord Adhesives Thermosetâ„¢ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-809 is a long working life, heat curing, two component epoxy formulation. It was designed especially for potting high voltage automotive ignition coils. The combination of low viscosity, exc..
Glass Transition Temp, Tg 95.0 °C
203 °F
wet
Henkel Hysol EA 9895 WPP Peel Ply
Pre-impregnated, polyester peel ply product supplied in film form. Specially designed resin system capable of curing at 350°F / 177°C. Compatible with state-of-the-art composite prepreg resin ..
Glass Transition Temp, Tg 95.0 °C
203 °F
Lucite International Elvacite ® 4045 Acrylic Resin
Elvacite® 4045 is a medium molecular weight methyl methacrylate polymer. It is designed for use in solvent based screen printing inks, but can be used in a variety of ink formulations.Information..
Glass Transition Temp, Tg 95.0 °C
203 °F
DSC
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive
TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive
TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor..
Glass Transition Temp, Tg 95.0 °C
203 °F
DMA
Hexcel® HexPly® ES/EH 84 120°C Curing Epoxy Matrix
HexPly® ES/EH 84 matrix is a structural epoxy resin for tubular parts designed for low pressure curing in the manufacture of sports goods and for industrial applications. It is ideal for the follow..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive
TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lense..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond GA47-2LV Instrument Adhesive
TRA-BOND GA47-2LV low viscosity adhesive is designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids. TRA-BOND GA47-2LV a..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive
TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system ..
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Tra-Con Tra-Bond F131 High Tg Room Temperature Cure Fiber Optic Adhesive
TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus ..
Glass Transition Temp, Tg >= 95.0 °C
>= 203 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind..
Glass Transition Temp, Tg >= 95.0 °C
>= 203 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i..
Glass Transition Temp, Tg >= 95.0 °C
>= 203 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:..
Glass Transition Temp, Tg >= 95.0 °C
>= 203 °F
Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy
Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif..
Glass Transition Temp, Tg 95.0 °C
203 °F
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive
EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl..
Glass Transition Temp, Tg 95.0 °C
203 °F
ASTM D-4065
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod..
Glass Transition Temp, Tg 95.0 °C
203 °F
Atom Adhesives AA-BOND F131 Epoxy Adhesive
AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical ..
Glass Transition Temp, Tg 95.0 °C
203 °F
cured
Atom Adhesives AA-BOND F156 Epoxy Adhesive
AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opa..
Glass Transition Temp, Tg 95.0 °C
203 °F
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating
3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri..
Glass Transition Temp, Tg 95.0 - 108 °C
203 - 226 °F
Average value: 102 °C Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Glass Transition Temp, Tg 95.0 °C
203 °F
Lucite International Elvacite ® 2021 Acrylic Resin
Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provide..
Glass Transition Temp, Tg 95.0 °C
203 °F
Lucite International Elvacite ® 2021E Acrylic Resin
Elvacite® 2021E is a high molecular weight methyl methacrylate. It provides a balance of solubility and hardness. It is used in migration barrier top coating for vinyl substrates. It is also used t..
Copyright © lookpolymers.com All Rights Reserved