Material Notes:
TRA-BOND GA47-2LV low viscosity adhesive is designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids. TRA-BOND GA47-2LV adhesive has a coefficient of thermal expansion that approximates that of aluminum, within normal temperature range.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
Mixed
Viscosity 50000 cP
50000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Adhesive Bond Strength 13.8 MPa
2000 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
Below Tg
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 95.0 °C
2.00 hour

@Temperature 203 °F
240 min

@Temperature 75.0 °C
4.00 hour

@Temperature 167 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Color Green
Working Life minutes 30
At 25°C