Polimeri Europa EDISTIR N1671 Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa EDISTIR N1671 Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection molding of items with complex and medium thick walls. Applications: Typical uses are domestic appliances, stationery, cutlery, housewares and medical articles.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 5.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.0 MPa
6090 psi
5 mm/min
Elongation at Break 2.0 %
2.0 %
5 mm/min
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min
Charpy Impact Unnotched 1.00 J/cm²
4.76 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
Vicat Softening Point 94.0 °C
201 °F
50°C/hr; 50N
Glass Transition Temp, Tg 95.0 °C
203 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Manufacturer specifies 'transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 70.0 kV/mm
1780 kV/in
Dissipation Factor 0.00020

@Frequency 100 Hz
0.00020

@Frequency 100 Hz
Comparative Tracking Index 400 V
400 V