Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electrical motor stator and rotors, to adhere copper foil to B-staged epoxy in the manufacture of printed circuits, and to coat, protect, and utilize coils and electronic subassemblies.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 19.5 - 23 %
19.5 - 23 %
Viscosity 40 - 80 cP
40 - 80 cP
Mechanical Properties Metric English Comments
Shear Strength 34.5 MPa
5000 psi
Overlap, Tap Water 30 days @ RT; ASTM D1002-72
34.5 MPa
5000 psi
Overlap, 20% Salt Spray 30 days @ 35°C; ASTM D1002-72
34.5 MPa
5000 psi
Overlap, 7 days at RT; ASTM D1002-72
34.5 MPa
5000 psi
Overlap, Aromatic Fuels 7 days @ RT; ASTM D1002-72
2.07 MPa

@Temperature 150 °C
300 psi

@Temperature 302 °F
Overlap; ASTM D1002
8.27 MPa

@Temperature 120 °C
1200 psi

@Temperature 248 °F
Overlap; ASTM D1002
24.1 MPa

@Temperature 82.0 °C
3500 psi

@Temperature 180 °F
Overlap; ASTM D1002
34.5 MPa

@Temperature -55.0 °C
5000 psi

@Temperature -67.0 °F
Overlap; ASTM D1002
34.5 MPa

@Temperature 24.0 °C
5000 psi

@Temperature 75.2 °F
Overlap; ASTM D1002
Peel Strength 1.75 kN/m
10.0 pli
T-Peel; ASTM D1876
Thermal Properties Metric English Comments
CTE, linear 262 µm/m-°C

@Temperature -20.0 - 70.0 °C
146 µin/in-°F

@Temperature -4.00 - 158 °F
543 µm/m-°C

@Temperature 100 - 120 °C
302 µin/in-°F

@Temperature 212 - 248 °F
Glass Transition Temp, Tg 95.0 °C
203 °F
Flash Point -14.0 °C
6.80 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+15 ohm-cm
1.20e+15 ohm-cm
Dielectric Constant 5.2

@Frequency 1000 Hz
5.2

@Frequency 1000 Hz
Dielectric Strength 94.5 kV/mm
2400 kV/in
Dissipation Factor 0.011

@Frequency 1000 Hz
0.011

@Frequency 1000 Hz
Descriptive Properties Value Comments
Appearance Light Amber