Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 160 - 175 °C | 320 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman |
|||
Melting Point | 160 - 175 °C | 320 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Indium Corp. Indalloy® 204 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches Semi-crystalline low melt polyester sheath/PET core. Luster: Semi-Dull. Finish: HydrophilicApplications of bicomponent polyester fiber: Absorbent products, FDA-compliant products, non-wovens, fi.. |
|||
Melting Point | 155 - 175 °C | 311 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Melting Point | 122 - 175 °C | 252 - 347 °F | |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | ASTM D789 |
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Melting Point | 145 - 175 °C | 293 - 347 °F | DSC; ASTM D3418 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | ISO 11357 |
Polyram PlusTek PD305G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced Nylon 12 for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polyram PlusTek RD101 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polyram PlusTek PD100 Nylon 12, Injection Molding Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | |
Polyram PlusTek PD300G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | ISO 11357 |
Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced Nylon 12 for injection molding applications. UL listed.Information provided by Polyram. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | ISO 11357 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 138 - 175 °C | 280 - 347 °F | Average value: 155 °C Grade Count:9 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | ASTM D789 |
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |