Material Notes:
30% Glass-fiber reinforced Nylon 12 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Water Absorption at Saturation 1.2 %
1.2 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Flexural Strength 180 MPa
26100 psi
ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Maximum Service Temperature, Air 100 °C
212 °F
Continuous use
145 °C
293 °F
Short peaks operation
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in