Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
30% Glass-fiber reinforced Nylon 12 for injection molding applications. UL listed.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Tensile Modulus 6.00 GPa
870 ksi
ISO 527
Flexural Strength 160 MPa
23200 psi
ISO 178
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in