Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extruded. PEARLTHANE® 12K92A is used for the extrusion of films in general and especially adhesive films, either flat or blown films.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength 35.06 MPa
5085 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.01100 GPa
1.595 ksi
ASTM D412
300% Modulus 0.0220 GPa
3.19 ksi
ASTM D412
Tear Strength 120 kN/m
685 pli
ASTM D624 (Die C)
Abrasion 25
25
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
MQSA 111
Glass Transition Temp, Tg -13.9 °C
7.00 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Zone 1 150 - 180 °C
302 - 356 °F
Zone 2 160 - 190 °C
320 - 374 °F
Zone 3 170 - 200 °C
338 - 392 °F
Zone 4 175 - 205 °C
347 - 401 °F
Die Temperature 175 - 200 °C
347 - 392 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44