Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 162 - 168 °C | 324 - 334 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1180 Bicomponent PP/PET Fiber Type - 3 Denier X 1.5 Inches 40/60 PP Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenier.. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | DSC |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Melting Point | 160 - 168 °C | 320 - 334 °F | DSC |
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF) Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope.. |
|||
Melting Point | 158 - 168 °C | 316 - 334 °F | ASTM D3418 |
Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2) Description: D-1 PVDF Powder has good solubility in some solvent, it is more suitable for lithium ion battery industry as binder. D-1 PVDF is a homopolymer with high dielectric constant, which shows.. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 220 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 520 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 526 N30 Polypropylene Homopolymer Improved rigidity, high durabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 532 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 220 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 310 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 N30 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50218 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50245 Polypropylene Homopolymer For electroplatingInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50258 Polypropylene Copolymer For electroplatingInformation provided by Addiplast. |
|||
Melting Point | 161 - 168 °C | 322 - 334 °F | |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 470 ST14 Polypropylene Copolymer Soft touchInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50284 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 210 Polypropylene Homopolymer UnreinforcedInformation provided by Addiplast. |
|||
Melting Point | 145 - 168 °C | 293 - 334 °F | Average value: 161 °C Grade Count:8 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Melting Point | 160 - 168 °C | 320 - 334 °F | Average value: 164 °C Grade Count:47 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |